atomic layer deposition

Deposition

A film-growth technique that exposes the wafer to alternating, self-limiting precursor pulses, depositing the film one atomic layer at a time. Because each cycle saturates, ALD delivers angstrom-level thickness control and perfectly conformal coverage of high-aspect-ratio structures, at the cost of slow deposition rates.